The morphologies of titanium layer after LIFT process, a a bump under pulse energy of 2 μJ, spot size of 45 μm, titanium with thickness of 160 nm, b a broken bump under pulse energy of 2 μJ, spot size of 45 μm, titanium with thickness of 100 nm, c a spot with shrank edge under pulse energy of 2 μJ, spot size of 45 μm, titanium with thickness of 80 nm, d a spot completely ablated under pulse energy of 2 μJ, spot size of 45 μm, titanium with thickness of 40 nm