Skip to main content

Table 2 Counted cell numbers on given timepoints. Polystyrene showed highest proliferation rates followed by PLA and titanium

From: In-vitro evaluation of Polylactic acid (PLA) manufactured by fused deposition modeling

 

Polystyrene

Titanium

Polylactic acid

Day 1

1.8 ± 0.1 × 104

1.3 ± 0.1 × 104

2.7 ± 0.5 × 104

Day 3

3.8 ± 0.5 × 104

1.9 ± 0,04 × 104

4.6 ± 5.6 × 104

Day 7

12.4 ± 1.5 × 104

2.7 ± 1,0 × 104

5.8 ± 1.1 × 104

Day 10

36.3 ± 0.9 × 104

10.4 ± 3.8 × 104

15.5 ± 1.1 × 104