Table 1 Characterization of produced nanofibers in different composition

From: Fabrication of chitosan-polyvinyl alcohol and silk electrospun fiber seeded with differentiated keratinocyte for skin tissue regeneration in animal wound model

Composition Mean diameter (nm) Pore size (μm) Porosity (%)
PVA 842 ± 205 1.33 ± 0.49 74 ± 3.9
Ch-PVA 1070 ± 340 0.9 ± 0.31 52 ± 4.7